Incoloy 825 Corrosion Resistance: Evaluating Acid and Chloride Service

Facebook
Twitter
Reddit
LinkedIn

Last updated:

Incoloy 825 corrosion resistance makes the alloy a candidate for sulfuric acid, phosphoric acid and chloride-bearing service. The useful limit depends on the fluid, temperature, type of attack and condition of the metal. A grade name alone cannot establish a safe operating temperature.

Does the published test describe your process? This guide shows how to match acid data to a duty. It also explains which records to request before you specify the metal. The complete Incoloy 825 guide provides broader grade background.

Key takeaways

  • Separate average metal loss from pits, crevice attack and cracking.
  • Match the test fluid, temperature, air exposure and impurities before comparing rates.
  • Keep standard 825 data separate from results for modified alloy variants.
  • Check the delivered and welded condition as well as the grade designation.

Illustrative scenario: a plant has clean make-up acid and a recycled acid stream at the same nominal strength. The recycled stream carries extra salts and solids. Both have the same acid strength. That does not mean they expose the metal to the same risk.

No measured outcome is assumed in this example.

For a material inquiry, list the fluid, acid strength, known impurities and normal and upset temperatures. Add the grade and product form. Use the grade guide’s inquiry route to share that duty sheet. This gives the reviewer facts to work with; it does not assume grade approval.

What Incoloy 825 corrosion resistance data measure

Incoloy 825 Corrosion Resistance at a Glance
Incoloy 825 Corrosion Resistance at a Glance

Identify the damage before reading the rate

A rate in mm/year describes metal loss in a stated test. It does not answer every damage question. A low average loss can still leave a question about a deep pit, attack under a gasket or a stress-related crack.

The Special Metals alloy 825 bulletin treats general corrosion, local attack and stress corrosion cracking as distinct concerns. Keep them separate when you assess a vessel, tube or fitting.

Concern Evidence to look for Question it does not settle alone
General metal loss Rate with fluid, exposure and test duration Whether a crevice will suffer local attack
Pitting Named solution, pH, temperature and method Whether a stressed component will crack
Crevice corrosion Crevice geometry and exposure conditions Performance of every joint design
Stress corrosion cracking Fluid, stress, temperature and exposure time Freedom from pitting or uniform loss

Use the table to choose the next question. Don’t use it to rank grades. If a report measures weight loss only, ask what test covers local damage in the planned part.

Check alloy identity and condition

Standard alloy 825 is UNS N08825, also identified as material number 2.4858. Special Metals lists nickel at 38.0-46.0%, molybdenum at 2.5-3.5%, copper at 1.5-3.0% and titanium at 0.6-1.2% by weight. Those ranges define the chemistry. They do not set a corrosion rate.

The bulletin links nickel with resistance to chloride stress corrosion cracking. Nickel, molybdenum and copper help the alloy resist reducing acids. Chromium helps it resist oxidizing media. Molybdenum also helps against pits and crevice attack.

Titanium, with suitable heat treatment, helps protect against sensitization. That is a change that can leave the metal’s grain boundaries open to attack.

Our Incoloy 825 properties guide expands the composition and property background. Chemistry helps explain how the metal behaves. It can’t replace a test matched to the process. Record the product form and heat treatment with the grade.

Incoloy 825 corrosion resistance in sulfuric acid

Read the named curve and its conditions

An isocorrosion curve links acid strength and temperature at a stated rate of metal loss. It can help you screen a duty when the test details match. The curve does not set one safe limit for all service.

For a concrete example, Alleima’s Sanicro 41 datasheet identifies the product with Alloy 825. Its Figure 1 compares Sanicro 41 and AISI 316L in deaerated sulfuric acid. The caption defines the curves as 0.1 mm/year, rounded in the source to 4 mpy. Keep that product name and fluid with the result.

Read a source plot in this order:

  1. Confirm the exact alloy or producer product and the test solution.
  2. Check whether concentration is a weight percentage and which temperature scale is used.
  3. Read the curve’s rate criterion and the conditions stated in its caption.
  4. Compare those conditions with normal operation, excursions and contaminants in your process.
  5. Identify the remaining differences before seeking a project acceptance decision.

Don’t replace the curve with a claim that every acid strength is safe below one temperature. That drops the link the plot was drawn to show. A test on one product form also does not approve every welded part.

Match air exposure and impurities

Alleima warns that oxygen content changes how sulfuric acid attacks the metal. It describes acid in contact with air as more corrosive than deaerated acid. You can’t use that warning to claim that air always improves 825’s performance.

The Special Metals aqueous corrosion handbook also makes acid chemistry and test details part of grade selection. Keep each source’s details together. Don’t join a rate from one test, a temperature from a second and a fluid from a third to create a new limit.

Source detail Record for your duty Why the comparison matters
Deaerated test acid Air contact and dissolved oxygen information The chemical environment can differ
Defined acid concentration Normal and upset concentration, with units The point on the plot may change
Named test solution Chlorides, other acids and dissolved species A mixed stream is a different exposure
Defined rate criterion Project loss and local-damage criteria An average rate is not full acceptance

When a quote cites a rate, ask for the plot and the test fluid. Mark what is unknown. If no one has measured the chloride level, don’t enter zero on the duty sheet.

For a first review, put the cited curve and duty sheet side by side. If the source says deaerated acid while the process has air contact, mark the match as incomplete. Do the same for an unknown impurity level. You have found a gap to resolve, not proved that the alloy will fail.

Keep the original test reference with that note. A later reviewer can then see why the curve was used, which part of the duty it covers and where more data are needed. This avoids turning an initial screen into a final design decision.

Check arithmetic without inventing a limit

Illustrative scenario: an engineer receives a note marked “150” beside a temperature. The original record must establish whether it means Fahrenheit or Celsius. If it means 150 °F, the conversion is (150 – 32) × 5/9 = 65.56 °C.

That is a unit conversion. It does not show that 825 will suit either duty.

Rate units need the same care. One mil is 0.0254 mm, so 5 mpy equals 0.127 mm/year. That is not exactly the 0.1 mm/year criterion in the Alleima caption.

Keep the rate shown by each source. The two figures are not the same design limit.

Phosphoric acid: pure solutions and wet-process evidence

Incoloy 825 Phosphoric Acid: Pure vs Wet Process
Incoloy 825 Phosphoric Acid: Pure vs Wet Process

Describe the actual acid stream

Pure and commercial phosphoric acid need separate review. The name “wet-process acid” does not fully define a fluid. The Special Metals handbook explains how impurities matter and why published rates can differ. Check the clean acid and the process stream against their own test data.

Start with an acid sample that represents the duty. Record acid strength, chloride, fluoride, residual sulfuric acid and solids where present. Note where and when the sample was taken. Don’t use fresh-feed data as if they describe the outlet of an evaporator or a surface under deposits.

For the two streams in the opening example, the next step is to collect those missing facts. You can’t yet say which grade will last longer. The process name and acid strength leave that question open.

Keep laboratory evidence in its proper role

Table 8 in the handbook is explicitly labeled laboratory corrosion tests in pure phosphoric acid. Nearby prose refers more broadly to lab and plant results. Keep the table’s own label when you use a row. It is lab data, not a customer case.

Copy the grade, acid strength, temperature, exposure, test duration and rate units together. Add what the source says about impurities. If a needed detail is absent, mark it as unavailable. Don’t borrow it from the next row.

A broad claim of good resistance does not erase differences between test rows. If the prose and a table seem to disagree, go back to the test details. Those passages do not establish one phosphoric acid limit or a service life.

Compare alternatives on matching evidence

The producer bulletin supports considering 825 for phosphoric acid service. It does not establish that a copper-phosphate film makes it superior to Inconel 625 in every such duty. An explanation about alloy chemistry does not replace matched test data.

The 825 versus 625 comparison is further reading on the two grades. For an actual selection, request evidence for the same fluid, damage mechanism and material condition. Keep purchase-price questions separate from the question of corrosion suitability.

Preparing an acid-service inquiry? Add the impurity assay, sampling location and exposure details to the initial duty sheet. Label measured values and estimates.

Then the reviewer knows which gaps to close. A request to approve “phosphoric acid service” alone does not show those gaps.

Chlorides: separate pitting, crevice corrosion and SCC

A crack result does not prove resistance to pits

Stress corrosion cracking, or SCC, involves a susceptible material, stress and a corrosive environment. Pitting and crevice corrosion are separate local-attack questions. Resistance to one mechanism cannot be treated as immunity to the others.

Alleima separates these results in its datasheet. Figure 2 concerns critical pitting temperatures in 3% NaCl at different pH values. Figure 3 concerns SCC testing in 40% CaCl2 at 100 °C and pH 6.5.

Those tests use different salts and ask different damage questions. Neither salt level sets a chloride limit for every plant stream.

Keep the full fluid name and method with each result. A “chloride test” label is too broad. Does it cover the pH, temperature, stress and shape of your part?

Check joints, deposits and excursions

Illustrative scenario: a reviewer compares a freely exposed coupon with a gasketed joint. The joint includes a tight crevice that the open coupon does not reproduce. The reviewer needs data for that crevice. This example does not predict a failure or its timing.

Producer guidance treats pits and crevice attack as separate concerns. List gaskets, overlaps, deposits, flow changes and stagnant periods for the seawater or brine part. Include cleaning and upset conditions in the duty. Then check which of these the cited test covers.

The sources used here do not set one seawater temperature cutoff. A pitting resistance equivalent number, or PREN, cannot predict service life on its own. It compares aspects of alloy chemistry. It does not describe every fluid, surface or joint.

Where a drawing includes crevices, make them visible in the evidence request. Ask which test geometry addresses them. If the report covers only an open surface, keep that limit visible in the review.

A practical comparison sheet can have one column for the test and one for the duty. Enter pH, salt identity, temperature, stress and the presence of a crevice in both. Leave unknown fields blank and mark them as open questions. This is a way to organize the review, not a new corrosion test or a prediction of failure.

Distinguish standard 825 from 825 CTP

VDM’s Alloy 825 CTP page identifies the variant as UNS N08827, material number 2.4861. Standard 825 is N08825/2.4858. The page describes increased molybdenum and enhanced pitting resistance for CTP.

Do not transfer a CTP seawater claim or PREN value to standard 825. Check the designation on the cited result and the material being offered. A suffix can mean a different chemistry. Check it before you compare results.

Turn corrosion screening into a fabrication and purchase evidence package

Stacked metal plates
Stacked metal plates

Write down the fluid and exposure

A useful material request separates facts from open questions. Two reviewers should be able to read the same duty sheet without guessing what the missing fields mean.

Part of the request Useful information
Process fluid Acid or salt identity, concentration basis and impurity analysis
Operating range Normal temperature and concentration, start-up and upset conditions
Exposure Immersion, vapor or splash; flow, stagnation and deposits
Component Product form, dimensions, joints and stressed locations
Material state Grade, heat identification, delivery condition and fabrication history
Acceptance basis Applicable project specification, damage criteria and required evidence

For mixed acids, organic acids, alkalis or flue gas desulfurization equipment, define the actual stream in the same way. The process label does not let you reuse an acid curve or chloride test without checking it. Each added fluid needs its own supporting data.

Include the fabricated condition

The VDM Alloy 825 datasheet covers processing alongside corrosion behavior. Together with the Special Metals bulletin, it shows why the metal’s condition matters. Chemistry alone does not describe the final part.

Record forming, welding and subsequent treatment relevant to the project. Use the Incoloy 825 welding guide for the separate fabrication discussion. This overview does not set a welding procedure or heat treatment for every product form. Use the project requirements and the applicable producer guidance.

Separate identity from service acceptance

A material test report helps document what was supplied. It cannot establish performance in every acid or chloride environment. Keep three questions separate: is it the right grade, does it meet the product standard, and will it meet the service criteria?

Use the Incoloy 825 specifications guide when preparing the product and documentation requirements. Ask for applicable test methods and acceptance criteria explicitly. Avoid prescribing one intergranular, pitting or cracking test to every duty without checking its scope.

Return to the two acid streams. Record each stream’s chemistry and exposure, even if both requests name N08825. State who will supply the missing process data and review the final service criteria. That makes the handoff useful without claiming that the grade is already approved.

Incoloy 825 corrosion resistance FAQ and next step

What is the maximum temperature in sulfuric acid?

There is no single maximum for every acid strength and duty in the sources reviewed here. Read the curve, its rate, fluid and air exposure together. Match those details to your duty. A temperature alone leaves the question open.

Why do impurities matter in phosphoric acid?

Pure-acid data do not fully describe a stream with other acids, halides or solids. The Special Metals handbook discusses these effects and why rates differ. Get the stream analysis and sampling point before using a rate. The process name does not supply those facts.

Does chloride SCC resistance make 825 suitable for seawater?

It addresses only part of the question. Pitting, crevice corrosion, stress, surface condition and exposure also need review. Keep the distinct test solutions in Alleima’s figures attached to their results. A crack-resistance result alone cannot approve a gasketed seawater assembly.

Is 825 unsuitable for all nitric acid service?

No. Special Metals describes resistance to oxidizing substances including nitric acid. In Alleima Table 1, Sanicro 41 in 50 wt% boiling nitric acid at 115 °C has a reported rate of 0.04 mm/year. This is a named producer result under stated conditions, not a grade-wide rate.

They don’t approve every acid strength or temperature. Ask for data for the actual fluid. A blanket yes or no drops those details.

What corrosion rate should I use for a delivered batch?

There is no single rate for every batch and process. Start with a test that matches the fluid, temperature, duration and state of the metal. Review general loss and local attack on their own terms. A batch record confirms the metal’s identity, but can’t create missing service data.

What should go into the next inquiry?

Prepare the grade and form, fluid analysis, operating range, joint details, fabricated condition and required acceptance evidence. Identify unknowns plainly. Use the Incoloy 825 grade guide as the inquiry starting point and attach that duty sheet.

Incoloy 825 corrosion resistance matters when the data answer the service question. Match the test to the process. Resolve the gaps before grade approval.

Our Alloy Materials
Recently Posted
Scroll to Top
Get in touch with us
Leave a message
Contact Form Demo